Mangalam Metal is a well-known exporter and manufacturer of Inconel Alloy 625 Round Bars, which is used for fasteners and instrumentation parts, along with in oil field applications. The addition of niobium in Inconel Alloy 625 Square Bars acts with the molybdenum to stiffen the alloy’s matrix and provide high strength without a strengthening heat treatment. The sluggish precipitation hardening response of Inconel Alloy 625 Flat Bars allows it to be readily welded without hardening or cracking. Hot-cold working for Inconel Alloy 625 Threaded Barsin the range 1700 Degree F / 1850 Degree F (927 Degree C / 1010 Degree C) will improve the strength of the forging if the service temperature is below about 1100 Degree F (593 Degree C). Inconel Alloy 625 Hollow Bars is used in Fasteners and instrumentation parts, Nuclear fuel element spacers, Hot extrusion tooling, Down hole shafting and strength bolting, etc.
Turbine engines and aircraft are the most common places where Inconel Alloy 625 Hexagonal Bars can be found, but it is very useful for many different types of machinery. Inconel Alloy 625 Triangular Bars is often used in Gas turbine engine parts, Firearms production, Liquid fuel rocket motor components, Springs, fasteners, Cryogenic tanks, etc. Also known as "heat-resistant super-alloys" or "high-temperature alloys", Inconel Alloy 625 Hex Bars can withstand severe mechanical stresses and strains in extreme environments while remaining stable, corrosion and creep resistant.
Grade | Inconel Alloy 625 / UNS NO6625 |
Specification | EN, DIN, JIS, ASTM, BS, ASME, AISI |
Standard | ASTM B446 / ASME SB446 |
Size | 5 mm To 500 mm |
Diameter | 0.1 mm to 100 mm |
Length | 100 mm To 3000 mm Long & Above |
Finish | Black, Bright Polished, Rough Turned, NO.4 Finish, Matt Finish, BA Finish |
Form | Round Bars, Square Bars, Flat Bars, Threaded Bars, Hollow Bars, Hexagonal Bars, Triangular Bars |
STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
Inconel 625 | 2.4856 | N06625 | NCF 625 | NA 21 | ХН75МБТЮ | NC22DNB4M | NiCr22Mo9Nb |
Grade | C | Mn | Si | Cu | S | Fe | Mo | Ni | Cr |
Inconel 625 | 0.10 max | 0.50 max | 0.50 max | – | 0.15 min | 5.0 max | – | 58.0 min | 20.0–23.0 |
Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
8.4 g/cm3 | 1.350 °C (2460 °F) | Psi – 1,35,000 , MPa – 930 | Psi – 75,000 , MPa – 517 | 42.5 % |