Hastelloy C276 Round Bars

UNS N10276 Round Bar, DIN 2.4819 Rods

Mangalam Metal is a prominent exporter of Hastelloy Alloy C276 Round Bars, which can be welded in either the annealed or the age condition. While most works available on precipitation have been performed at temperatures below the salvos for Hastelloy C276 Bright Bars, it appeared of interest to also investigate the case where phase precipitates directly from the matrix free of precipitates. In recent decade there is a growing demand for cost efficient and eco-friendly machining for Hastelloy C276 Flat Bars, many researcher are taking keen interest in development of more advance machining processes. The ease and economy of Hastelloy C276 Hex Bar can be fabricated, combined with good tensile, fatigue, creep, and rupture strength, have resulted in its use in a wide range of applications. UNS N10276 Round Bar is developed for high-temperature, high-pressure, highly-oxidative environments in a rocket engine.

Uniform reductions during forging of Hastelloy C276 Hexagonal Bars will prevent the formation of a duplex grain structure. Typical short time tensile properties of DIN 2.4819 Rods as a function of temperature are shown here for material solution treated and aged. Hastelloy C276 Forged Bars has highly resistant to chloride and sulfide stress corrosion cracking. Hastelloy C276 Rods is one of the most widely used alloys in the aerospace industry, heavily featured in engines, turbines, and heat exchangers. Welding of Hastelloy C276 Rods in the aged condition will cause the formation of a softened heat-affected zone.

Specification Of Hastelloy C276 Round Bars

Standards : ASTM B574, ASME SB574
Dimensions : EN, DIN, JIS, ASTM, BS, ASME, AISI
Wire : Thickness starting from 0.05mm
Round bar size : Diameter: 3-~800mm
Hex Bar size : 2-100mm A/F
Flat bar size : Thickness: 2 -100mm / Width: 10 to 500mm
Square bar size : 4 to 100mm
Rectangular Bars Size : 33 x 30mm to 295 x 1066mm
Hollow Bar : 32mm OD x 16mm ID to 250mm OD x 200mm ID
Tolerance : H8, H9, H10, H11, H12, H13K9, K10, K11, K12 or as per clients’ requirements
Finish : Black, Bright Polished, Rough Turned, NO.4 Finish, Matt Finish, BA Finish

Equivalent Grades

STANDARD WERKSTOFF NR. UNS JIS EN GOST OR
Hastelloy C276 2.4819 N10276 NW 0276 NiMo16Cr15W ХН65МВУ  ЭП760

Chemical Composition

Grade C Mn Si Co P Fe Mo Ni Cr S W V
Hastelloy C276 0.010 max 1 max 0.08 max 2.5 max 0.04 max 4 – 7 15 – 17 Bal 14.5-16.5 0.03 max  3.0-4.5 0.35 max

Mechanical Properties

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.89 g/cm3 1370 °C (2500 °F) Psi – 1,15,000 , MPa – 790 Psi – 52000 , MPa – 355 40%